MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dow Dow™ DPDA-3152 NT7 MDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: Product Description: Dow DPDA-3152 NT7 medium density polyethylene resin is produced via UNIPOL™ process technology from Dow and is intended for rotational and injection molding. It is specifically designed for applications requiring excellent processability and aesthetics combined with low warpage and good mechanical properties. Processing and Stabilization: DOW DPDA-3152 NT 7 MDPE Resin is fully heat and UV stabilized resulting in a wide processing latitude, good color retention and long life expectancy.
  • Rotational molding or injection molding
  • For intermediate bulk containers, toys, general purpose custom molding, agricultural storage tanks, water tanks, marine parts, indoor consumer articles
  • Excellent impact strength, stress crack resistance and processability
  • Long term UV stabilization: UV-8 stabilizer package
Complies with: US FDA 21 CFR 177.1520©3.1a; Canadian HPFB No Objection; Underwriters Laboratories Inc; NSF International NSF/ANSI Std 61 (sec 4 & 5). Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: US FDA 21 CFR 177.1520©3.1a; EU No 10/2011; NSF STD-61: UL

Form: Pellets

Processing Method: Injection Molding; Rotational Molding

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.937 g/cc0.0339 lb/in³ASTM D792
ESCR 100% Igepal® >= 1000 hour
@Temperature 50.0 °C
>= 1000 hour
@Temperature 122 °F
F50; ASTM D1693
ESCR 10% Igepal® >= 982 hour>= 982 hourF50; ASTM D1693
Melt Flow 5.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 18.8 MPa2720 psiASTM D638
Flexural Modulus 0.655 GPa95.0 ksi1% Secant; ASTM D790B
Impact Test  >= 80.0 J
@Thickness 3.17 mm,
Temperature -40.0 °C
>= 59.0 ft-lb
@Thickness 0.125 in,
Temperature -40.0 °F
Rotational Molded
 >= 255 J
@Thickness 6.35 mm,
Temperature -40.0 °C
>= 188 ft-lb
@Thickness 0.250 in,
Temperature -40.0 °F
Rotational Molded
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 °C257 °F
Deflection Temperature at 0.46 MPa (66 psi) 51.7 °C125 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 35.0 °C95.0 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF489 / 311182

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.