MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507

Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, Insulation Bags, Multi-Wall Liners, Coextruded Film Structures

Film properties below based on film thickness of 20 µm.

Data provided by Chevron Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.939 g/ccASTM D1505
Environmental Stress Crack Resistance >= 2000 hour
@Temperature 50.0 °C
F50, Cond. B.; ASTM D1693
Melt Flow 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
High Load Melt Index 21 g/10 min
@Load 21.6 kg,
Temperature 190 °C
High Load Melt Index; ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 31.0 MPaASTM D638
Tensile Strength, Yield 21.0 MPaASTM D638
Film Elongation at Break, MD 370 %ASTM D882
 580 %ASTM D882
Elongation at Break >= 800 %Molded; ASTM D638
Flexural Modulus 0.660 GPa3 pt. secant. ASTM D790
Secant Modulus, MD 0.410 GPaASTM D882
Secant Modulus, TD 0.480 GPaASTM D882
Elmendorf Tear Strength, MD 30.0 g/milNotched; ASTM D1922
Elmendorf Tear Strength, TD 690 g/milASTM D1922
Dart Drop 7.50 g/micronF50; 1.5 in. dart/26 in. drop height; ASTM D 1709
Film Tensile Strength at Break, MD 48.0 MPaASTM D882
Film Tensile Strength at Break, TD 28.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 121 °CASTM D1525
Brittleness Temperature <= -59.0 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUTENE-H BE0350 HDPE
Eastman M3018-P Polyethylene
DuPont 20 Series 2020 Specialty Polyethylene Resin
Aaron Industries AVPE HD 300-3 MELT 20 Virgin Polyethylene

PCHEVV69 / 20465

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.