Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request. Key Features and Benefits: - Designed to replace first generation 350°F (176°C) cure systems.
- Wide cure temperature process window of 250°F to 350°F
- Exhibits very low void content, i.e., <2% after vacuum cure.
- Superior fiber property translation.
- 180°F Wet service temperature after ~250°F cure
- Good tack and drape characteristics for 3 weeks at room temperature
Applications/Qualifications: - Primary Aircraft Structures
- Fuselage
- Wing
- Control Surfaces
- Secondary Aircraft Structures
- Aircraft Frames
- Doors
- Shelves
- Bulkheads
Information provided by Park Electrochemical Corp. |