MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik DH40 Cemented Carbide for Woodworking  (discontinued **)
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite; Nonferrous Metal; Tungsten Alloy

Material Notes:
  • The unique grain size distribution is optimized to improve the toughness and the micro crack resistance
  • The composition of the DH grades includes specific additions to increase the thermal resistance (thermal cycling fatigue), and the corrosion/oxidation resistance
  • This combination of innovations gives the DH grades a high edge retention and crack resistance. These properties, combined with a good brazeability and grindibility, allow the DH grades family to be very efficient when looking at cost/performance ratio.

    Features:

  • Medium grain size
  • Moderate to medium abrasion resistance
  • High impact strength
  • Binderphase content 11%
  • Codes: ISO K40

    Information provided by Sandvik

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 14.35 g/cc0.5184 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell A 8989
    Hardness, Vickers 1280128030
    Fracture Toughness 16.0 MPa-m½14.6 ksi-in½

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    ASTM A131 Steel, grade EH36
    Sandvik H10F Cemented Carbide for Woodworking
    ASTM A131 Steel, grade DH36
    Sandvik C9M Cemented Carbide for Can Tooling
    MMCC Al/SiC 3DP Particulate Aluminum Matrix Composite

    NSANDV039 / 18933

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.