MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Versalis EDISTIR N1670 Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Symbol according to ISO 1043-1: PS
Designation: Thermoplastic ISO 1622-PS,E,095-06

General purpose polystyrene with good flow and good heat resistance. Recommended for extrusion in blend with HIPS or clear SBS for thermoformed packaging.

Applications: Food packaging articles as drink and dairy cups, plates, trays.

Unfilled. Suitable for Sheet Extrusion, Thermoforming. Supplied as pellets.

ISO data. Information provided by Enichem

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/cc
Melt Flow 5.4 g/10 min
@Load 5.00 kg,
Temperature 200 °C
cm³/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 42.0 MPa5 mm/min
Elongation at Break 2.0 %5 mm/min
Tensile Modulus 3.28 GPa1 mm/min
Charpy Impact Unnotched 1.00 J/cm²
Charpy Impact, Notched 0.200 J/cm²
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
Dielectric Constant 2.5
@Frequency 100 Hz
Dielectric Strength 70.0 kV/mm
Dissipation Factor 0.00020
@Frequency 100 Hz
Comparative Tracking Index 400 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
Vicat Softening Point 94.0 °C50°C/hr; 50N
Glass Transition Temp, Tg 95.0 °C10°C/min test
Flammability, UL94 HB
@Thickness 1.50 mm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Manufacturer specifies 'transparent' but doesn't quantify.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis EDISTIR N1460 Polystyrene
Total PSC 500 Polystyrene
Stratasys® ABS
Röchling Formaterm® PS-HI sign/advertising
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded

PENI52 / 35859

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.