MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Versalis EDISTIR N1670 Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Symbol according to ISO 1043-1: PS
Designation: Thermoplastic ISO 1622-PS,E,095-06

General purpose polystyrene with good flow and good heat resistance. Recommended for extrusion in blend with HIPS or clear SBS for thermoformed packaging.

Applications: Food packaging articles as drink and dairy cups, plates, trays.

Unfilled. Suitable for Sheet Extrusion, Thermoforming. Supplied as pellets.

ISO data. Information provided by Enichem

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Melt Flow 5.4 g/10 min
@Load 5.00 kg,
Temperature 200 °C
5.4 g/10 min
@Load 11.0 lb,
Temperature 392 °F
cm³/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 42.0 MPa6090 psi5 mm/min
Elongation at Break 2.0 %2.0 %5 mm/min
Tensile Modulus 3.28 GPa476 ksi1 mm/min
Charpy Impact Unnotched 1.00 J/cm²4.76 ft-lb/in²
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm
Dielectric Constant 2.5
@Frequency 100 Hz
2.5
@Frequency 100 Hz
Dielectric Strength 70.0 kV/mm1780 kV/in
Dissipation Factor 0.00020
@Frequency 100 Hz
0.00020
@Frequency 100 Hz
Comparative Tracking Index 400 V400 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C180 °F
Vicat Softening Point 94.0 °C201 °F50°C/hr; 50N
Glass Transition Temp, Tg 95.0 °C203 °F10°C/min test
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Manufacturer specifies 'transparent' but doesn't quantify.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis EDISTIR N1460 Polystyrene
Total PSC 500 Polystyrene
Stratasys® ABS
Röchling Formaterm® PS-HI sign/advertising
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded

PENI52 / 35859

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.