MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polymer Resources ABS-G25 ABS, 25% Glass Reinforced
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled

Material Notes: Acrylonitrile Butadiene Styrene, 25% Glass Reinforced

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cmASTM D955
Melt Flow 0.50 - 5.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 13500 psiASTM D638
Tensile Strength, Yield 13500 psiASTM D638
Elongation at Yield 1.5 %ASTM D638
Flexural Strength 18500 psiASTM D790
Flexural Modulus 1100 ksiASTM D790
Izod Impact, Notched 1.00 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 230 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 375 - 390 °F
Middle Barrel Temperature 410 - 430 °F
Front Barrel Temperature 410 - 440 °F
Melt Temperature 410 - 460 °F
Mold Temperature 120 - 140 °F
Drying Temperature 175 - 185 °F
Dry Time 3.00 - 4.00 hour
Vent Depth 0.00100 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES HiFill® ABS GF30 30% Glass Filled
RTP Company RTP 604  Acrylonitrile Butadiene Styrene (ABS) Glass Fiber 25%
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
Lotte Advanced Materials Starex® GA-4025 ABS, 25% Glass Filled
Cheng Yu Plastic A703G25 ABS 25% Glass Fiber Reinforced

PPOLYQ005a / 160518

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.