MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Vinnapas® EP 7000 Vinyl Acetate Ethylene
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product description: VINNAPAS® EP7000 is a poly(vinyl alcohol) stabilized vinyl acetate-ethylene (VAE) copolymer dispersion with a glass transition temperature (Tg) of approximately - 3 °C. It was developed as a high performance, ultrahigh solids dispersion offering superior adhesion, wet tack and setting speed over conventional VAE dispersions.

Properties: VINNAPAS® EP7000 is manufactured to an ultra-high solids content of 70 percent while maintaining a viscosity range of 1200-2700 mPa.s. This combinationof high solids and moderate viscosity allows formulators to prepare very unique high solids products. This dispersion provides excellent wet tack, speed of set, machining characteristics, film clarity and adhesion. The dry film of VINNAPAS® EP7000 is tackier, clearer and more water resistant than standard grade VAE dispersions. VINNAPAS® EP7000 does not thicken excessively onthe addition of plasticizers, fillers or dispersible powders. Despite its high solids content, it can be applied on high-speed packaging machines using roll, extrusion or spray application equipment. VINNAPAS® EP7000 is produced without the use of any surfactants or defoamers that contain alkylphenol ethoxylates (APEOs). No formaldehyde or formaldehyde donors are intentionally added.

Application: VINNAPAS® EP7000 can be used in numerous applications. For high-performance vinyl laminations, the product provides excellent adhesion, heat resistance and aesthetics with less warpage and reduced grain raise in wood-based substrates than standard solids dispersions. In clear film overprint laminations, VINNAPAS® EP7000 dispersion yields excellent film clarity and water resistance. For construction applications, VINNAPAS® EP7000 provides the high filler acceptance needed to produce high-solids adhesives. VINNAPAS® EP7000 can also be used in bottle labeling, bookbinding, and high speed packaging applications where its rheology and very fast setting speeds and extremely high wet tack offer unique performance characteristics.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/cc
Solids Content 69.5 - 71.5 %
pH 4.5 - 5.5
Brookfield Viscosity 1200 - 2700 cP3 @ 20 rpm
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -3.00 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zeon Specialty Materials ZEONEX® K26R Cyclo Olefin Polymer
Wacker Vinnapas® EF 104 Vinyl Acetate Ethylene
Wacker Vinnapas® 400 H Vinyl Acetate-Ethylene Copolymer
OGC OKP-1 Polyester Optical Plastic
Zeon Specialty Materials ZEONEX® E48R Cyclo Olefin Polymer

PWACK9650 / 205179

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.