MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman Pentalyn™ 750-HV-M Rosin Resin
Categories: Polymer

Material Notes: Product Description: Pentalyn™ 750 HV-M rosin resin is a phenolic modified resin ester with high viscosity, excellent gloss and good release of solvents, which makes it recommendable mainly for rotogravure inks in aromatic solvents.

Application/Uses:

  • Graphic Arts
  • Hot Melt Adhesives
  • Solventborne Adhesives
Key Attributes:
  • Excellent gloss
  • Good release of solvents
  • High viscosity

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 20[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 159 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 10
 
Descriptive Properties
AppearanceCrystalline Solid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Phenolic; Unreinforced; Molded
Covestro Bayhydrol® XP 2418 Polyurethane Coating

PEATM5491 / 222685

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.