MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Armacell OleTex® BDJN 200 EVA/LDPE Foam
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Polyethylene (PE); Low Density (LDPE)

Material Notes: Armacell LLC (South Holland, IL Plant) manufactures a closed cell, 2 lb/ft3 (32 kg/m3) density, general purpose, EVA/LDPE fine cell foam product BDJN 200 in bun form, with a nominal 25% compression strength deflection value of 6 psi. BDJN 200 is a chemically cross-linked polyolefin product that is available in a variety of colors and has been fully tested to the physical property test methods listed in ASTM D 3575. BDJN 200 does not incorporate an added flame retardant but meets FMVSS-302 at thicknesses of 0.250” (1/4”) (6.35 mm) and higher.
  • Widely used general purpose EVA/LDPE blend, an industry standard
  • ASTM D 3575 tested polyolefin, closed cell material
  • Fine cell – manufactured in blocks (buns)
  • BDJN 200H is UL listed to UL 94 HF-1

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 lb/ft³ASTM D3575W
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 47.0 psiASTM D3575T
Elongation at Break 240 %ASTM D3575T
Compressive Strength 5.70 psi
@Strain 25 %
ASTM D3575D
Tear Strength 11.0 pliASTM D3575G
Compression Set 20 %ASTM D3575B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °F
Minimum Service Temperature, Air -65.0 °F
 
Descriptive Properties
FlammabilityFMVSS302Pass at >6.35 mm
 HF-1Pass at >1.5 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Armacell OleTex® BCJN 200 EVA/LDPE Foam
Armacell OleTex® BKJN 200 LDPE Foam
Celanese Ateva® 1241 EVA polymer for compounds, flexible packaging and foam
ExxonMobil Escorene® LD-728 High EVA Resin
Braskem Evateno® 3019 PE EVA Foam Copolymer

PARMD115 / 186726

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.