MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Hipscon™ B-515 Static Control Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: Hipscon™ B-515 is a carbon black-filled, Polystyrene compound available in compound form. Hipscom™ B-515 compound maintains extremely low gloss surfaces after molding, allowing for easy reading of package contents via automated sensors.

Features:

  • High degree of stiffness
  • Consistent, permanent ESD protection
  • Humidity independent

Applications:

  • Electronic component packaging and handling trays
  • Material handling boxes and bins

Data provided by Noveon, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.1 MPa3500 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Tensile Modulus 1.86 GPa270 ksiASTM D638
Flexural Modulus 1.86 GPa270 ksiASTM D790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 ohm-cm1.00e+7 ohm-cmASTM D257
Surface Resistivity per Square <= 1e+05<= 1e+05ASTM D257
Static Decay <= 0.010 sec<= 0.010 secFTMS-101C; 12% R.H., (+5000 V to 50 V)
 <= 0.010 sec<= 0.010 secFTMS-101C; 12% R.H., (-5000 V to -50 V)
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C178 °FASTM D648
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOVEON00 / 55264

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.