MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Nucrel® 30907 Ethylene Acid Copolymer Resin
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Nucrel® 30907 is an ethylene acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resin. This resin may also be used in conventional blown and cast film extrusion and coextrusion equipment.

Characteristics:

  • Excellent adhesion to unprimed foil.
  • Excellent adhesion to coextruded nylon.
  • For superior structure reliability and barrier integrity.
  • Very good hot tack, sealability through contamination, and heat seal strength for strong, reliable heat seals.
  • Lower melt index than Nucrel® 3990 to increase melt strength and to minimize neck-in during extrusion coating operation
  • Applications:

  • Sealants for sachets in both food and non-food applications.
  • Toothpaste tubes as a foil/LDPE tie layer.
  • Other foil-containing pouches and sachets.
  • Medical/pharmaceutical packaging.
  • Cable shield wrap.
  • Information provided by DuPont™

    This former DuPont product line is now a Dow product line.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.940 g/ccASTM D792
    Melt Flow 7.0 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    ASTM D1238
     
    Thermal PropertiesOriginal ValueComments
    Melting Point 83.0 °CFreezing Point, DSC; ASTM D3418
     98.0 °CDSC; ASTM D3418
    Vicat Softening Point 77.0 °CASTM D1525
     
    Processing PropertiesOriginal ValueComments
    Rear Barrel Temperature 135 °CBlow Film
     175 °CExtrusion Coating
    Middle Barrel Temperature 175 °CBlow Film
     260 °CExtrusion Coating
    Front Barrel Temperature 180 °CBlow Film
     290 °CExtrusion Coating
    Die Temperature 356 °FBlow Film
     554 °FExtrusion Coating
    Casting Temperature 9.00 °C

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Dow Nucrel® 3990L Ethylene Acrylic Acid
    Dow Nucrel® 30705 Ethylene Acrylic Acid
    Dow Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating
    Dow Primacor® 3460 Ethylene Acrylic Acid (EAA)
    Dow Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film

    PDUP960 / 33527

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.