DANCOLL_W155 is an aqueous, soft aliphatic polyurethane dispersion with good crosslinking characteristics. This product achieves dry films without thermoplasticity. DANCOLL_W155 is used as a paint-, finish- and coating binder as well as a dispersion for textile impregnation and textile equipment. Application: DANCOLL_ W155 serves as a binder for paints, coatings, textile laminations and finishes. For the two component processing we are recommending the crosslinking with our aqueous crosslinker DANCURE 101. The tested applications of DANCOLL_ W155 are: - Textile impregnations and textile equipments
- Ground- and top coatings for leather- and textile coating.
- Leather binder blended with acrylate dispersion.
- PVC finishes, printing inks and synthetic coatings finishes.
- Mixings with DANCOLL_ 148-56 for textile finishes, especially for glazable
Information provided by Danquinsa GMBH |