MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Methyl phenyl ketone
Categories: Fluid; Solvent

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.032 g/cc
@Temperature 20.0 °C
0.03728 lb/in³
@Temperature 68.0 °F
Viscosity 1.8 cP
@Temperature 20.0 °C
1.8 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 120.151 g/mol120.151 g/mol
Vapor Pressure 0.000271 bar
@Temperature 20.0 °C
0.203 torr
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 38.5 bar28900 torr
Critical Temperature 428 °C802 °F
Critical Density 0.320 g/cc0.0116 lb/in³
Critical Molar Volume 376 cm³/mol22.9 in³/mol
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.064 J/g-°C
@Temperature 25.0 °C
0.2543 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Melting Point 19.7 °C67.5 °F
Boiling Point 201.8 °C395.2 °F
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.2384
Antoine's Vapor Pressure B Parameter3781.07
Antoine's Vapor Pressure C Parameter-81.15
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
Critical Compressibility (Zc)0.25
Dipole moment (p/C.m)1.001E-27
Molar Heat Capacity (298K)127.835 J/mol-K
Molar Heat Capacity of Vapor a Parameter-29.56
Molar Heat Capacity of Vapor b Parameter0.6406
Molar Heat Capacity of Vapor c Parameter-0.0004069
Molar Heat Capacity of Vapor d Parameter9.715E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

VORGS236 / 99600

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.