MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kohesi Bond KB 1452 HT-2CRAO Two component, room temperature curing, thermally conductive, cryogenic epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Product Highlights:
  • Very high thermal conductivity
  • Good flow properties
  • Castable up to 3 inches depth and more
  • Outstanding chemical resistance
  • Cryogenic serviceability
  • Capable of passing NASA low outgassing
Kohesi Bond KB 1452 HT-2CRAO is an exclusive two component epoxy system suitable for bonding, sealing, coating, potting and encapsulation applications. It has a favorable 100:40 (Part A: Part B) mix ratio by weight. It offers excellent thermal conductivity and an extremely low coefficient of thermal expansion (CTE). The optimal cure schedule is an overnight room temperature set-up followed by a heat cure at 70°C - 90°C for 3 - 5 hours. Rapid cures are achievable with a straight heat cure as well at elevated temperatures. KB 1452 HT-2CRAO offers an extensive service temperature range of 4K (-269.15°C) to +200°C. It offers outstanding physical strength properties and dimensional stability. KB 1452 HT-2CRAO adheres well to a wide variety of substrates including metals, ceramics, most plastics and glass. In addition to superior electrical insulation, it also offers excellent chemical resistance to a variety of organic and inorganic acids, solvents, alkali, aromatic hydrocarbons, oils and water. Additionally it is capable of passing NASA standards for low outgassing (ASTM E-595). Owing to its high thermal conductivity and cryogenic serviceability, KB 1452 HT-2CRAO is widely used in electronics, aerospace, semiconductor and various OEM applications.

Typical Applications:

  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors: Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 200 - 1000 cP200 - 1000 cPPart B
 50000 - 125000 cP50000 - 125000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 80>= 80
Tensile Strength >= 52.4 MPa>= 7600 psi
Tensile Modulus >= 3.52 GPa>= 510 ksi
Adhesive Bond Strength >= 8.96 MPa>= 1300 psiTensile Lap Shear, Al/Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.0 - 20.0 µm/m-°C8.33 - 11.1 µin/in-°F
Thermal Conductivity 1.40 - 1.50 W/m-K9.72 - 10.4 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -269 °C-452 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 90.0 °C
2.00 - 3.00 hour
@Temperature 194 °F
Option 2
 2880 - 4320 min
@Temperature 23.0 °C
48.0 - 72.0 hour
@Temperature 73.4 °F
Option 1
Working Life 75.0 - 125 min75.0 - 125 min100 g of mixed epoxy
Shelf Life 6.00 Month6.00 Monthin original unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOHESI946 / 249125

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.