MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Poco Graphite EDM-C200 EDM Graphite
Categories: Carbon; Graphite

Material Notes: POCO's EDM-C200 is a Superfine graphite infiltrated with copper which offers excellent metal removal rates and good wear resistance. EDM-C200 provides improved cutting stability in poor flushing conditions. EDM-C200 is an excellent material for cutting aerospace alloys.

Applications:
Aerospace exotic metal cutting
High quality roughing electrode
Structural ribs
Carbide Applications

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 10 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62
Flexural Strength 83.4 MPa
Compressive Strength 160 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000290 ohm-cm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Graphite, Carbon, C
NeoGraf eGRAF® HITHERM™ HT-1220 Graphite
CoorsTek CRB-300 General-Duty Carbon Graphite
Envalior TEPEX® dynalite 408-C200(2)-FG290(2)/45% Carbon – Filament Glass – TPU Consolidated Composite Laminate
Firestone C200-001 Nylon 6

CPOCO07 / 85584

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.