MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Silfoam® SD 860 Silicone Antifoam Agent
Categories: Fluid

Material Notes: SILFOAM® SD 860 is an anhydrous silicone antifoam agent that is well dispersible in water and based on organic components with a small amount of an organo-functional silicone fluid.

Application: Basically, SILFOAM® SD 860 is recommended for organic systems where a high compatibility with the antifoam agent must be ensured. SILFOAM® SD 860 can be used in applications which usually pose problems for silicones, e. g., paints, adhesives and water miscible cooling lubricants. In addition, SILFOAM® SD 860 exhibits excellent degassing properties in high solids content systems, e. g. concretes, mortars, and ceramic slurries.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccDIN 12791
Kinematic Viscosity 50 - 200 cStDIN 51562
 
Thermal PropertiesOriginal ValueComments
Flash Point 108 °CISO 2719
Ignition Temperature 315 °Cliquids; DIN 51794
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.446DIN 51423
 
Descriptive Properties
Active ingredients (%)100
Appearancecolorless, opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9448 / 204977

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.