MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LNP STARAMIDE P-1000 HI 020 Polyamide 6  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes:
  • Features: Impact Modified, High Impact Resistance
  • Forms: Pellets
  • Processing Method: Injection Molding

Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Linear Mold Shrinkage 0.019 - 0.021 cm/cm0.019 - 0.021 in/inISO294-4
Linear Mold Shrinkage, Transverse 0.019 - 0.021 cm/cm0.019 - 0.021 in/inISO294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psiISO 527-1, -2
Elongation at Break 100 %100 %ISO 527-1, -2
Tensile Modulus 1.80 GPa261 ksiISO 527-1, -2
Izod Impact, Notched (ISO) 44.0 kJ/m²20.9 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) 96.0 kJ/m²45.7 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C124 °FUnannealed; ISO 75A-1, -2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 252 - 266 °C486 - 511 °F
Mold Temperature 54.4 - 93.3 °C130 - 200 °F
Drying Temperature 82.2 °C180 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %Suggested
Back Pressure 0.172 - 0.345 MPa24.9 - 50.0 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shell Carilon® DP P1000 Polyketone
LG Chemical LUMID HI5006A(W) PA6/ABS, High Impact, Good Dimensional Stability
LG Chemical LUMID HI1102A(W) PA6, High Impact
EPICHEM PA 6 Polyamide 6
BASF Ultramid® 8202 L Intermediate PA6 (Dry)

PZLNP1279 / 51361

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.