MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT JAF 100 Silicone Defoamer
Categories: Other Engineering Material

Material Notes: Description: CHT USA's 100% active defoamers are formulated to control foam in a wide variety of industrial processes.

Key Features

  • Superior foam knockdown and defoaming persistence
  • Effective in low concentrations
  • Effective in hot and cold systems
  • Effective in high and low pH systems
Key Applications
  • Coatings
  • Oil and Gas
  • Pulp and paper
  • Waste water treatment
Application: JAF 100 is used in to control foam in industrial applications including paper, oil and gas and recycling. JAF series antifoams provide superior performance over a wide pH range.

Addition Rates
Dosage – 1: 100-10,000 ppm

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measure 4000 cSt4000 cSt
Storage Temperature <= 40.0 °C<= 104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
% actives1
AppearanceLiquid
ColorGrayish white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL239 / 314722

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.