MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman TXIB™ Formulation Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No. 6846-50-0

Product Description: Eastman TXIB™ Formulation Additive is the lowest viscosity (9 cps) additive available to the flexible PVC industry. Eastman TXIB™ Formulation Additive is completely compatible with PVC in all proportions and is usually blended with general-purpose plasticizers such as DOP or DOTP. The unique low viscosity makes this material particularly suitable for PVC plastisols and often allows adding additional fillers to the plastisol, resulting in a cost savings. Eastman TXIB™ Formulation Additive has efficiency generally equal to DOP, which makes substitution in a vinyl formulation very easy. It imparts a dry surface to the vinyl, excellent resistance to staining, and physical properties equivalent to DOP. Eastman TXIB™ Formulation Additive is also used in inks, coatings, urethane elastomers, and nail polish lacquers.

Application/Uses:

  • Automotive
  • Flexible PVC
  • Flooring/Interior surfaces
  • Food contact
  • Latex sealants
  • Medical
  • Peroxides
  • Polyurethane adhesives
  • PVAc water based adhesives
  • PVC plastisol sealant
  • PVC plastisols
  • VAE water based adhesives
Key Attributes:
  • Inert - Nonfood use

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.945 g/cc
Viscosity 9.0 cP
Vapor Pressure <= 0.0000147 atm
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.050
 
Thermal PropertiesOriginal ValueComments
Melting Point -70.0 °CFreezing Point
Boiling Point 281 °C
Flash Point 136 °CSetaflash Closed Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.43
 
Descriptive Properties
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5203 / 222397

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.