MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Addiplast Addinyl A2 E Flame Retardant Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Flame retardant, halogen free

Information provided by Addiplast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878Conditioned; ISO 868
 8585ISO 868
Tensile Strength, Yield 60.0 MPa8700 psiConditioned; ISO R 527
 85.0 MPa12300 psiISO R 527
Elongation at Break 30 %30 %ISO R 527
 >= 50 %>= 50 %Conditioned; ISO R 527
Modulus of Elasticity 1.30 GPa189 ksiConditioned; ISO 178
 2.90 GPa421 ksiISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²ISO 180/1A
 12.0 kJ/m²5.71 ft-lb/in²Conditioned; ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/IeU
 NBNBConditioned; ISO 179/IeU
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179/IeA
 1.10 J/cm²5.23 ft-lb/in²Conditioned; ISO 179/IeA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmConditioned; CEI 60093
 1.00e+15 ohm-cm1.00e+15 ohm-cmCEI 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmConditioned; CEI 60093
 1.00e+15 ohm1.00e+15 ohmCEI 60093
Dielectric Strength 28.0 kV/mm711 kV/inCEI 60243-1
Comparative Tracking Index >= 600 V>= 600 VCEI 60112/Solution A
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FISO 75-2/AF
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
Oxygen Index 28 %28 %ISO 4589
Glow Wire Test 960 °C1760 °FCEI 60695/2/1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural
Eurotec® Tecomid® NB40 GR30 NL XA60 PA6, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Epsan Eplamid 6 GX0 20 NC Q1C0B601 Polyamide 6, Halogen Free
Epsan Eplamid 6 GV0 20 NC Q1C0C001 Polyamide 6, Halogenated

PFADD915 / 156129

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.