MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Nouryon Trigonox K-84PG Cumyl hydroperoxide
Categories: Other Engineering Material

Material Notes: Trigonox K-84PG is an organic peroxide (84% active ingredient in aromatic solvent mixture) for Asymmetric Oxidation and other pharmaceutical synthesis reactions.

CAS number: 80-15-9

EINECS/ELINCS No: 201-254-7

Applications: Trigonox K-90PG may be used in chemical synthesis of medicines and fine chemicals to make personal care and pharmaceutical products. The high purity and extensive compliance controls make it a low risk reagent or late stage intermediate. It can be used in emulsion, solution and bulk reactions and reactions are used in many blockbuster drugs.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³
Half-life  0.100
@Temperature 195 °C
0.100
@Temperature 383 °F
[hr]
 1.00
@Temperature 166 °C
1.00
@Temperature 331 °F
[hr]
 10.0
@Temperature 140 °C
10.0
@Temperature 284 °F
[hr]
Viscosity 10.4 cP10.4 cP
Molecular Weight 152.2 g/mol152.2 g/mol
Storage Temperature -30.0 - 40.0 °C-22.0 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 65.0 °C149 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay82.0-86.0 %
Color= 200 Pt-Co
Content8.62-9.04 %Active oxygen
Content (%)10.51Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1201 / 286724

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.