MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Taro Plast Tarolon 2511 PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Polycarbonate medium viscosity, standard transparent grade for general purpose. Available: only transparent color, UV stabilized (L), release agent (W).

Information provided by Taro Plast S.p.a.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Water Absorption 0.12 %
@Time 86400 sec
ISO 62
Water Absorption at Saturation 0.35 %ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cmISO 2577
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 62.0 MPaISO 527
Elongation at Break 85 %ISO 527
Tensile Modulus 2300 MPaISO 527
Flexural Strength 80.0 MPaISO 178
Flexural Modulus 2500 MPaISO 178
Izod Impact, Notched 700 J/m127x12.7x3.2; ASTM D256
Charpy Impact Unnotched >= 300 kJ/m²
@Temperature 23.0 °C
80x10x4; ISO 179/1eU
 >= 300 kJ/m²
@Temperature -20.0 °C
80x10x4; ISO 179/1eU
Charpy Impact, Notched 30.0 kJ/m²80x10x4; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D257
Comparative Tracking Index 225 VMethod A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°CISO 11359
Maximum Service Temperature, Air 120 °C
@Time 72000 sec
IEC 60216
Hot Ball Pressure Test 135 °CIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 140 °CISO 75/A
Vicat Softening Point 150 °C
@Load 1.00 kg
ISO 306
Flammability, UL94 V-2
@Thickness 1.60 mm
127x2.17xThickness
Oxygen Index 26 %6.3x12.7x3.2; ASTM D2863
Glow Wire Flammability Index 850 °C
@Thickness 2.00 mm
60x60xThickness; IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTARO059 / 283167

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.