MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT Group QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent choice for the molding of intricate patterns, skin molding and applications where high durometer, dimensional stability and extremely tough rubber are required. A variety of catalysts are offered with this material.

Key Features:

  • Low specific gravity
  • Low viscosity
  • High tear strength
  • Long work-life
  • Fast demold time
  • Excellent dimensional stability
Main Applications:
  • Molds for large and small statues
  • Molds for polyester, polyurethane and epoxy resin castings
  • Molds for technical articles and prototype
  • Molds for furniture and picture frame replication
  • Molds for GFRC pre-cast

      Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccUncatalyzed, Moldmaster Green
 1.00 g/cc1.00 g/ccUncatalyzed, Moldmaster Blue
 1.00 g/cc1.00 g/ccUncatalyzed, Moldmaster Red
 1.13 g/cc1.13 g/cccatalyzed with Moldmaster Green
 1.13 g/cc1.13 g/cccatalyzed with Moldmaster Blue
 1.13 g/cc1.13 g/cccatalyzed with Moldmaster Red
 1.13 g/cc1.13 g/cccatalyzed with Moldmaster Purples
 1.16 g/cc1.16 g/ccUncatalyzed, Moldmaster Purple
Viscosity 100 cP100 cPUncatalyzed, Moldmaster Green
 150 cP150 cPUncatalyzed, Moldmaster Blue
 150 cP150 cPUncatalyzed, Moldmaster Red
 150 cP150 cPUncatalyzed, Moldmaster Purple
 28000 cP28000 cPcatalyzed with Moldmaster Green
 28000 cP28000 cPcatalyzed with Moldmaster Blue
 28000 cP28000 cPcatalyzed with Moldmaster Red
 28000 cP28000 cPcatalyzed with Moldmaster Purple
 35000 cP35000 cPBase
Linear Mold Shrinkage <= 0.0025 cm/cm<= 0.0025 in/incured 72 hrs @ RT
Storage Temperature <= 38.0 °C<= 100 °F6 months
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2323cured 72 hrs @ RT
Tensile Strength 3.40 MPa493 psicured 72 hrs @ RT
Elongation at Break 500 %500 %cured 72 hrs @ RT
Tear Strength 22.8 kN/m130 pliB, cured 72 hrs @ RT
 
Processing PropertiesMetricEnglishComments
Cure Time 200 - 400 min4 - 6 hourDemold time, catalyzed with Moldmaster Red
 240 - 360 min4.00 - 6.00 hourDemold time, catalyzed with Moldmaster Blue
 480 - 600 min8.00 - 10.0 hourDemold time, catalyzed with Moldmaster Green
 500 - 600 min8 - 10 hourDemold time, catalyzed with Moldmaster Purple
Tack-Free Time 120 - 240 min2.00 - 4.00 hourCatalyzed with Moldmaster Red
 120 - 240 min2.00 - 4.00 hourCatalyzed with Moldmaster Blue
 240 - 360 min4.00 - 6.00 hourCatalyzed with Moldmaster Purple
 240 - 360 min4.00 - 6.00 hourCatalyzed with Moldmaster Green
Pot Life 30.0 min30.0 mincatalyzed with Moldmaster Blue
 30.0 min30.0 mincatalyzed with Moldmaster Red
 60.0 min60.0 mincatalyzed with Moldmaster Purple
 60.0 min60.0 mincatalyzed with Moldmaster Green
 
Descriptive Properties
ColorBeigeBase
 BlueUncatalyzed, Moldmaster Blue
 Dark Purplecatalyzed with Moldmaster Purple
 GreenUncatalyzed, Moldmaster Green
 Light Bluecatalyzed with Moldmaster Blue
 Light Greencatalyzed with Moldmaster Green
 Light Redcatalyzed with Moldmaster Red
 PurpleUncatalyzed, Moldmaster Purple
 RedUncatalyzed, Moldmaster Red

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) CAF® 7037 Silicone Rubber
Elkem (Bluestar Silicones) CAF® 1 Extra Fluid Silicone Rubber
Momentive Performance Materials Silopren™ Electro 940 Liquid Silicone Rubber - Medium Voltage
Elkem (Bluestar Silicones) CAF® 99 AXAD BLACK Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ VRM-65 Hi-Pro Green Silicone Rubber

PACC062 / 22189

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.