MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Genioplast® Pellet P Plus Silicone Gum
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Silicone

Material Notes: Product description: GENIOPLAST® PELLET P PLUS is a pelletized silicone gum formulation with an outstanding high loading of ultrahigh molecular weight (uhmw) siloxane polymer.

Properties: GENIOPLAST® PELLET P PLUS does not contain any thermoplastic resin as a carrier but some quantity of fumed silica instead. Fumed silica as a constituent of the pelletized formulation does not show any adverse effect in the application; it provides general compatibility with thermoplastic resins when used as a compounding additive in thermoplastic systems to impart benefits such as processing improvements and modification of surface characteristics.

Special features: When added to thermoplastic resin systems at 0.1 % to 1 %, improved processing and flow of the resin is expected, including less extruder torque, less extruder die pressure, faster throughput, reduction of melt viscosity and better mould filling. At higher addition levels, 1 % to 5 %, also improved surface properties are expected, including lower coefficient of friction and greater mar and abrasion resistance. GENIOPLAST® PELLET P PLUS can also improve burning characteristics of polyolefins when applied in combination with halogen free flame retardant fillers. GENIOPLAST® PELLET P PLUS is expected to give improved benefits compared to conventional lower molecular weight additives, e.g. less screw slippage, long-term low coefficient of friction, fewer paint and printing problems, and a broader range of performance capabilities.

Application: Additive for:

  • polyolefin compounds
  • engineering plastics compounds
  • TPE compounds

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Appearancetranslucent, whitish pellets
Content (%)30Fumed silica
 70Siloxane polymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Genioplast® Pellet S Silicone Gum
Evonik Compound VS 100 Masterbatch
Evonik Compound VS 6000 Masterbatch
Evonik Compound VS 3000 Masterbatch
Wacker Genioplast® Pellet K Silicone Gum

PWACK9305 / 204834

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.