MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Elantas Conathane® CC-1195 (Conap) Polyurethane Two-component Dielectric Conformal Coating
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes:
Dielectric Conformal Coatings for Electronics
Cytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, instrumentation (industrial and military), missiles, spacecraft, fire and smoke detectors as well as coatings for electronic components, coils and transformers. And no small reason why -- all of the coatings described have been specifically formulated as dielectric insulating coatings to provide the user the ultimate protection available for his electronic assemblies; be it environmental (dirt, dust, humidity, fungus, temperature extremes, etc) or electrical insulation of conductors. These coatings are not designed for use as floor coatings or other general purpose uses; they have been produced under essentially "clean-room" conditions using raw materials with a minimum of ionizable impurities which would detract from their insulating qualities.

Cytec (Conap) CC-1195 Conathane® Polyurethane Two-component Dielectric Conformal Coating
  • Two Component
  • 100/70 Mix Ratio (by Weight)
  • Passes Thermal Shock Test (MIL-I-46058C)
  • Non-Nutrient Fungus Resistance (MIL-I-46058C)
  • Passes Flexibility Test (1/8" Mandrel Bend) (MIL-I-46058C)
  • Excellent Chemical and Solvent Resistance
  • Chemical Cure
Cure Type: Chemical

Information provided by Cytec, subsequently acquired by Elantas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 60 %
Viscosity 75 cP
@Temperature 25.0 °C
Initial mixed viscosity of components.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 6.00e+12 ohm-cmInsulation Resistance; Recovery, 24 hrs after 10-day Cycling (25°C, 50% Relative Humidity)
 2.50e+13 ohm-cmInitial Insulation Resistance (50% Relative Humidity)
 6.10e+10 ohm-cm
@Temperature 65.0 °C
Insulation Resistance During 10th day Cycling (95% Relative Humidity)
Dielectric Constant 3.42ASTM D150
Dielectric Strength 3000 V/milASTM D149
Dissipation Factor 0.016
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °F
Minimum Service Temperature, Air -65.0 °F
Flash Point 55.0 °F(TCC)
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 hour
@Temperature 60.0 °C
 10080 min
@Temperature 25.0 °C
Tack-Free Time 240 - 300 min
@Temperature 25.0 °C
Pot Life 240 - 360 min
@Temperature 25.0 °C
Shelf Life 12.0 MonthShelf Life Time at 25°C in original, unopened containers.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCYTEC09 / 29241

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.