MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Flint Hills AP5106-HA Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Features: Excellent impact stiffness balance, good mold release.

Applications: Compression and injection molding: caps and closures

Information Provided by Flint Hills Resources

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 5.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104ASTM D785
Tensile Strength, Yield 30.0 MPaASTM D638
Elongation at Yield 6.0 %ASTM D638
Flexural Modulus, 1% Secant 1517 MPaASTM D790
Izod Impact, Notched 107 J/m
@Temperature 23.0 °C
ASTM D256
Gardner Impact 9.00 J
@Temperature -30.0 °C
ASTM D5420
Tangent Modulus 1586 MPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 108 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Flint Hills AP5995-HA Polypropylene Impact Copolymer
Flint Hills AP5520-HA Polypropylene Impact Copolymer
Flint Hills AP6835-HS Polypropylene Impact Copolymer
Flint Hills P4C5B-181B Polypropylene Homopolymer
Flint Hills P6G4Z-097 Impact Copolymer Polypropylene

PFLINT013 / 104567

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.