MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Taiwan PU TPUE-UEH80 Extrusion Thermoplastic Polyurethane, High Hydrolysis Res. / Polyether Base For Making Tubes / Hoses
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Key features:
  • Polyester / Polyether base
  • Extrusion molding
  • Transparent pellet- Hardness: 80A-95A
  • Good wear resistance
  • High abrasion resistance
  • Good performance on elongation
Application:
  • 1. Air Bag, Cable & Wire, Belt, Film & Sheet and other extrusion parts.
  • 2. Hose Material: Air Tube, Hose, Fire Hose, Cable & Wire.
  • 3. Sheet Material: Film, Sheet, Conveyor Belt.

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080
Tensile Strength 22.6 MPa3270 psi
Elongation at Break 1000 %1000 %
100% Modulus 5.39 MPa782 psi
300% Modulus 7.85 MPa1140 psi
Abrasion 2020[mg]
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 °C347 °FCompression Zone
 180 °C356 °FMetering Zone
Feed Temperature 170 °C338 °F
Die Temperature 185 °C365 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTAIWPU095 / 305825

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.