MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Toray AMILAN™ CM1056K48 Nylon 6, 20% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Nylon 6, blow molding, high viscosity,GF20%, PA6-GF20.

General Amilan™ Notes: AMILAN™ nylon (polyamide) is a thermoplastic engineering plastic containing an amide group (-CONH-) and it exhibits excellent strength, toughness, heat resistance, and anti-friction wear resistance. A variety of grades designed for various customer needs and applications are available.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³Dry; ISO 1183
Water Absorption 6.5 %6.5 %In 23°C water, polymer initally dry; ISO 62
 1.2 %
@Time 86400 sec
1.2 %
@Time 24.0 hour
In 23°C water, polymer initally dry; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119
@Temperature 23.0 °C
119
@Temperature 73.4 °F
Dry; ISO 2039-2
Tensile Strength  45.0 MPa
@Temperature 80.0 °C
6530 psi
@Temperature 176 °F
2.5% Moisture Content; ISO 527-1,2
 55.0 MPa
@Temperature 80.0 °C
7980 psi
@Temperature 176 °F
Dry; ISO 527-1,2
 70.0 MPa
@Temperature 23.0 °C
10200 psi
@Temperature 73.4 °F
2.5% Moisture Content; ISO 527-1,2
 115 MPa
@Temperature 23.0 °C
16700 psi
@Temperature 73.4 °F
Dry; ISO 527-1,2
 165 MPa
@Temperature -40.0 °C
23900 psi
@Temperature -40.0 °F
2.5% Moisture Content; ISO 527-1,2
 190 MPa
@Temperature -40.0 °C
27600 psi
@Temperature -40.0 °F
Dry; ISO 527-1,2
Elongation at Break  2.5 %
@Temperature -40.0 °C
2.5 %
@Temperature -40.0 °F
Dry; ISO 527-1,2
 3.0 %
@Temperature 23.0 °C
3.0 %
@Temperature 73.4 °F
Dry; ISO 527-1,2
 3.0 %
@Temperature -40.0 °C
3.0 %
@Temperature -40.0 °F
2.5% Moisture Content; ISO 527-1,2
 4.0 %
@Temperature 80.0 °C
4.0 %
@Temperature 176 °F
Dry; ISO 527-1,2
 5.0 %
@Temperature 80.0 °C
5.0 %
@Temperature 176 °F
2.5% Moisture Content; ISO 527-1,2
 9.0 %
@Temperature 23.0 °C
9.0 %
@Temperature 73.4 °F
2.5% Moisture Content; ISO 527-1,2
Flexural Strength  100 MPa
@Temperature 23.0 °C
14500 psi
@Temperature 73.4 °F
2.5% Moisture Content; ISO 178
 175 MPa
@Temperature 23.0 °C
25400 psi
@Temperature 73.4 °F
Dry; ISO 178
Flexural Modulus  1.00 GPa
@Temperature 80.0 °C
145 ksi
@Temperature 176 °F
2.5% Moisture Content; ISO 178
 2.30 GPa
@Temperature 80.0 °C
334 ksi
@Temperature 176 °F
Dry; ISO 178
 2.60 GPa
@Temperature 23.0 °C
377 ksi
@Temperature 73.4 °F
2.5% Moisture Content; ISO 178
 3.40 GPa
@Temperature -40.0 °C
493 ksi
@Temperature -40.0 °F
2.5% Moisture Content; ISO 178
 5.20 GPa
@Temperature 23.0 °C
754 ksi
@Temperature 73.4 °F
Dry; ISO 178
 6.00 GPa
@Temperature -40.0 °C
870 ksi
@Temperature -40.0 °F
Dry; ISO 178
Charpy Impact Unnotched  1.15 J/cm²
@Temperature -40.0 °C
5.47 ft-lb/in²
@Temperature -40.0 °F
Dry; ISO 179
 2.70 J/cm²
@Temperature -40.0 °C
12.8 ft-lb/in²
@Temperature -40.0 °F
2.5% Moisture Content; ISO 179
Charpy Impact, Notched 0.650 J/cm²
@Temperature 23.0 °C
3.09 ft-lb/in²
@Temperature 73.4 °F
V-Notched. Dry; ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FDry; DSC Method
Deflection Temperature at 0.46 MPa (66 psi) 214 °C417 °FDry; ISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 184 °C363 °FDry; ISO 75-1,2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY9152 / 248841

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.