MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT Group EP IS EPI Engineered Polymers Integral Skin Flexible Foam
Categories: Polymer; Thermoset

Material Notes: EP-IS is integral skin flexible foam, “Powered by Reactamine ® Technology”, designed to give excellent surface skin. EP-IS contains cyclopentane as its blowing agent, which conforms to EPA standards for no CFC or HCFC blowing agents. Density can be varied from 5 – 30 PCF to obtain different hardness in the finished product.

Part of the Amber Chemical Group. Data provided by manufacturer.

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 25 - 6525 - 65Dependent on mold density.
Tensile Strength 1.08 - 1.27 MPa157 - 184 psi
Elongation at Break 70 - 90 %70 - 90 %
Tear Strength 3.93 - 5.89 kN/m22.4 - 33.6 pli
 
Processing PropertiesMetricEnglishComments
Mold Temperature 37.8 - 57.2 °C100 - 135 °F
Cure Time 3 - 4.02 min0.05 - 0.0670 hourDemold Time
Tack-Free Time 0.583 - 1.25 min0.00972 - 0.0208 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase Multi-Flex® A 2504LC TPE Thermoplastic Elastomer
Northstar Polymers MPG-A25A Room-Temperature Curable Liquid Castable Polyurethane
Northstar Polymers MPA-A30B Mold-Making Resin
General Plastics LAST-A-FOAM® FR-3803 FST Polyurethane Foam
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer

PACC085 / 22212

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.