MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Teknor Apex APEX® 310 Flexible Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Oil Resistant

Uses:Flexible Cord Jacketing; Liquid Tight Conduit Jacketing

Wire Types:SJT; SRDT; ST

Agency Rating:UL 360

Form: Pellets

Processing Method: Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 87
@Time 15.0 sec
87
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 19.2 MPa2780 psiASTM D638
 19.2 MPa
@Treatment Temp. 37.8 °C,
Time 605000 sec
2780 psi
@Treatment Temp. 100 °F,
Time 168 hour
Oven Aged; UL 1581
 19.6 MPa
@Treatment Temp. 15.6 °C,
Time 605000 sec
2840 psi
@Treatment Temp. 60.0 °F,
Time 168 hour
ASTM #2 Oil; UL 1581
Elongation at Break 340 %340 %ASTM D638
 269 %
@Treatment Temp. 15.6 °C,
Time 605000 sec
269 %
@Treatment Temp. 60.0 °F,
Time 168 hour
ASTM #2 Oil; UL 1581
 340 %
@Treatment Temp. 37.8 °C,
Time 605000 sec
340 %
@Treatment Temp. 100 °F,
Time 168 hour
Oven Aged; UL 1581
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °FContinuous; ASTM D794
Brittleness Temperature -24.0 °C-11.2 °FASTM D746
Oxygen Index 25 %25 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 °C360 °F
 
Descriptive Properties
AppearanceOpaque
Temperature Rating80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0175 / 236666

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.