MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Albis Plastics Polypropylene A 12 H-GF20 20% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Semi-crystalline Polypropylene Homopolymer (PPHP)

Characteristics: General Purpose: Medium Stiffness and Toughness

Applications: Appliances, Furniture, Cases, Packaging and Novelties

Processing: Injection Molding (Melt Temperature: 425-575°F, Mold Temperature: 65-160°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ASTM D792
Melt Flow 5.5 g/10 min5.5 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 44.8 MPa6500 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Modulus of Elasticity 4.10 GPa595 ksiASTM D638
Flexural Yield Strength 60.0 MPa8700 psiASTM D790
Izod Impact, Notched 0.370 J/cm0.693 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 134 °C273 °FASTM D648
Vicat Softening Point 105 °C221 °F(VST/B/50); ASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 218 - 302 °C424 - 576 °FInjection
Mold Temperature 18.0 - 71.0 °C64.4 - 160 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® PP GF20 CC HF 20% Glass Filled
LG Chemical LUPOL HI2202B PP+GF20%, High Impact
LG Chemical LUPOL GP2200 PP+GF20%
Celanese Celstran® PP-GF20-23 AF3001 Natural PP, 20% Glass Reinforced
Albis Plastics Polypropylene PP 14A3 GF20 20% Glass Fiber

PZA1B99 / 21786

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.