MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Silres® KX Silicone Resin
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: SILRES® KX is a methyl group containing silicone resin solution in xylene.

Properties: SILRES® KX is typically used in heat resistant coatings. It combines outstanding heat resistance and weatherability. With proper coating formulation, thermal stability up to 600°C (1100°F) can be achieved in combination with suitable temperature stable pigments and fillers.

Special features:

  • good balance of flexibility, hardness, heat resistance and curing speed
  • very low viscosity
  • air-drying
  • limited compatibility (preferably used as a sole binder)
  • excellent hydrophobicity and corrosion-protection
Application: SILRES® KX is suitable for all kinds of heat-resistant paints. It is an excellent choice for (anti-corrosion) coatings on mufflers, exhaust systems, engine parts, boilers, furnaces, ovens and oven inserts, chimneys, barbeques and electric and gas heaters, incinerators. At temperatures above 250°C (480°F) the organic groups of silicone resins start to degrade. After all the organic parts of the silicone resin have been pyrolytically decomposed, the product that remains moves to an inorganic stoichiometric composition of (SiO2)n. It is this layer which firmly binds pigments and fillers to the coated substrate.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³DIN 51757
Solids Content 49 - 51 %
@Treatment Temp. 200 °C,
Time 3600 sec
49 - 51 %
@Treatment Temp. 392 °F,
Time 1.00 hour
Kinematic Viscosity 6.0 - 12 cSt6.0 - 12 cStDIN 51562
 
Thermal PropertiesMetricEnglishComments
Flash Point 24.0 °C75.2 °FDIN 51755
Ignition Temperature 465 °C869 °FDIN 51794
 
Descriptive Properties
Appearanceclear, colorless to slightly yellow solution

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9576 / 205105

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.