MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil 32 Mobil DTE Excel Series
Categories: Fluid; Lubricant

Material Notes: Mobil DTE Excel Series oils are supreme performance hydraulic oils developed for use in high-speed, high-pressure piston, vane and gear pumps. They are formulated from high quality base stocks and specially selected super-stabilised additives. Their advanced technology ashless anti-wear additive system was developed to give exceptional corrosion protection for copper-based alloys in severe hydraulic applications such as high-pressure axial piston pumps. This unique additive system also gives the Mobil DTE Excel Series excellent compatibility with coolants used in metal working applications. The Mobil DTE Excel Series oils exhibit excellent oxidation and thermal stability properties which results in extended oil and filter life while providing optimum equipment protection reducing both maintenance and product disposal costs. They were developed in conjunction with the major OEMs to meet the stringent requirements of severe hydraulic systems using high pressure, high output pumps as well as handling the critical requirements of other hydraulic system components such as close clearance servo-valves and the high accuracy numerically controlled (NC) machine tools. They are designed to work with systems operating under moderate to severe conditions where high levels of anti-wear and film strength protection are needed, yet they are formulated to work where non-anti-wear hydraulic oils are generally recommended.

Hydraulic systems critical to deposit build-up such as sophisticated Numerically Controlled (NC) machines, particularly where close clearance servo-valves are used; Systems employing multi-metal designs in pumps and other system components; Applications where cross-contamination of hydraulic fluids and coolants can occur; High pressure vane, piston and gear pumps; Systems where very high operating temperatures are typical; Where small amounts of water are unavoidable; In systems containing gears and bearings; Systems requiring a high degree of load-carrying capability and anti-wear protection; Applications where thin oil-film corrosion protection is an asset such as in systems containing moisture

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.8725 g/cc
@Temperature 15.0 °C
0.03152 lb/in³
@Temperature 59.0 °F
ASTM D4052
Viscosity Measurement 9797Index; ASTM D2270
 
Thermal PropertiesMetricEnglishComments
Pour Point -33.0 °C-27.4 °FASTM D97
Flash Point 222 °C432 °FASTM D92
 
Descriptive Properties
Copper Strip Corrosion1A3 hrs @ 100°C
Foam Sequence I, ASTM D90220/0
Foam Sequence II, ASTM D89320/0
Foam Sequence III, ASTM D89320/0
FZG Gear Test, DIN 51534, Fail Stage12
Rust Prevention, Synthetic Sea WaterpassASTM D665B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient OnFlex™ U 5370A-E0077 Thermoplastic Elastomer (TPE)
Covestro Texin® DP7-1157 Thermoplastic Polyurethane + ABS Blend
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy
Avient Versollan™ RU 2204X Thermoplastic Elastomer (TPE)
Avient Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE)

WEXXON082 / 75507

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.