MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mallard Creek Polymers Rovene® 6014 Acrylic Emulsion
Categories: Polymer

Material Notes: Applications: Rovene® 6014 is a self crosslinking acrylic polymer providing a stiff hand to frothed or saturated substrates. Rovene® 6014 is recommended for various nonwoven and paper applications requiring a stiff hand with resistance to heat and light aging. Rovene® 6014 also provides good wet strength and chemical resistance.

Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 6014 Material Safety Data Sheet before handling, storing, or using this product.

Information provided by Mallard Creek Polymers

Key Words: paper
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 45 - 46 %
Particle Size 0.18 µm
pH 3.0 - 5.0
Brookfield Viscosity <= 200 cP#2/20 rpm
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 30.0 °C
 
Descriptive Properties
EmulsifiersAnionic
Residual Monomer0.09% Max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hardwire 12x-23-12 High Density Composite
Akro-Plastic Akromid® B3 GF 30 S1 (2091) PA66/6 Dry, 30% Glass Filled
Dynasol Calprene® 540 Thermoplastic Rubber SBS Dry
Touchstone CFOAM® 20 Structural Carbon Foam
Mallard Creek Polymers Rovene® 6015 Acrylic Emulsion

PMCP008 / 104665

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.