MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Airkool HP 2-Cycle Motor Oil
Categories: Fluid; Lubricant

Material Notes: 76® Airkool HP 2-Cycle Motor Oil is a premium quality, low-ash, API TC engine oil specially formulated for use in high-output commercial chain saws, motorcycles and other air-cooled 2-stroke cycle gasoline engines. It may be used in either direct oil injection or premix engines. Airkool HP 2-Cycle Motor Oil has a high level of detergency to help minimize piston ring sticking and exhaust port deposits to maintain good power output in 2-stroke cycle engines. It has excellent lubricity to protect against piston and cylinder scuffing, and helps reduce spark plug fouling and preignition problems. It is pre-diluted with a high-flash solvent for easy mixing with gasoline at low temperatures for premix applications. Airkool HP 2-Cycle Motor Oil meets JASO FD and ISO-L-EGD low-smoke requirements.

Applications:

  • High-output commercial chain saws that operate at 17,000-20,000 rpm
  • Motorcycles, scooters and all-terrain vehicles (ATVs)
  • Lawn-care equipment (mowers, weed trimmers, leaf blowers)
  • Other air-cooled 2-stroke cycle gasoline engines where an API TC oil is specified
Airkool HP 2-Cycle Motor Oil meets or exceeds the requirements of:
  • API Service TC
  • ISO-L-EGD
  • JASO FD, FC, FB
Features/Benefits:
  • Low-ash formulation helps minimize engine deposits and preignition
  • High detergency helps minimize piston ring sticking and reduce exhaust port blocking
  • Protects against piston and cylinder scuffing
  • Reduces spark plug fouling
  • Excellent rust and corrosion protection
  • Meets JASO FD low-smoke requirements
  • Keeps engine parts clean
  • Mixes easily with gasoline at low temperatures for premix applications
  • Dyed for easy visibility when mixed with gasoline
  • Suitable for either direct oil injection or premix engines

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.858 g/cc
Density 7.14 lb/gal
Viscosity Measurement 147Index
Kinematic Viscosity at 40°C (104°F) 48.4 cSt
Kinematic Viscosity at 100°C (212°F) 8.3 cSt
Ash 0.11 %Sulfated; ASTM D874
 
Thermal PropertiesOriginal ValueComments
Pour Point -40.0 °C
Flash Point 73.0 °CPMCC
 78.0 °CCOC
 
Descriptive Properties
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability
LyondellBasell Astryn 73A6-3 Polypropylene Copolymer, 30% Calcium Carbonate
LG Chemical LUMAX IN-5001 High Impact PBT
Petromont 1201 High Density Polyethylene Resin
LyondellBasell Lupolen 4261 A HDPE, Blow Molding Grade

WCON5019 / 198272

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.