MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AlphaGary PVC 2212RHT/1-118 CLEAR 080X Polyvinyl Chloride Thermoplastic
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded; PVC, Transparent

Material Notes: High melt flow and excellent heat stability and radiation resistance for fistulas, hubs, connectors, drip chambers, etc.
Formulated for injection molding or extrusion

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 77
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Clear; thickness not specified
 
Descriptive Properties
DEHP FreeYes
Phthalate FreeYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AlphaGary PVC 2212/7-118 CLEAR 0003 Polyvinyl Chloride Thermoplastic
AlphaGary PVC 2212/S-110 CLEAR 0003 Polyvinyl Chloride Thermoplastic
AlphaGary PVC 2212C2B/H-118 CLEAR 0003 Polyvinyl Chloride Thermoplastic
AlphaGary PVC 2212-100 CLEAR 0003 Polyvinyl Chloride Thermoplastic
Dow HDPE 25455N High Density Polyethylene

PGARY9960 / 140746

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.