MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Addiplast Addilene H 420 K24 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: High density

Information provided by Addiplast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.40 g/cc0.0867 lb/in³ISO 1183/A
Melt Flow 10 g/10 min10 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8181ISO 868
Tensile Strength at Break 10.0 MPa1450 psiISO R 527
Tensile Strength, Yield 12.0 MPa1740 psiISO R 527
Modulus of Elasticity 4.50 GPa653 ksiISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 1.50 J/cm²7.14 ft-lb/in²ISO 179/IeU
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179/IeA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index >= 600 V>= 600 VCEI 60112/Solution A
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 - 168 °C329 - 334 °FISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FISO 75-2/AF
Vicat Softening Point 153 °C307 °FISO 306/A50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 199 X 108940 C Polypropylene (PP), High Gravity Compound
Polyram RamOfin PPC371B73 Polypropylene, 73% Mineral Filled
Polyram RamOfin PPC370B73 Polypropylene, 73% Mineral Filled
Polyram Metal Cap PPC373B72 Polypropylene, 72% mineral Filled
Polyram Metal Cap PL380Z81 Heavy Density Polyethylene, 81% Mineral Filled

PFADD817 / 156031

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.