MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Admiralty, Antimonial, Copper Alloy, UNS C44500, OS025 Temper, Tube
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Nominal Grain Size 0.025 mm

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Spot Weld, Butt Weld; Fair Suitability – Gas Shielded Arc Welding, Capacity for Being Hot Formed

Common Fabrication Processes: Bending; Forming; Machining

Typical Uses: Condenser Tubes; Condenser Tube Plates; Distiller Tubes; Evaporator Tubing; Ferrules; Heat Exchanger Tubing; Strainers

Applicable Specifications: Condenser & Heat Exchanger Tube with Integral Fins – Seamless B359/B359M, Welded ASTM B956, with Integral Fins ASME B359, ASME B956/B956M; Heat Exchanger Tube – Welded ASTM B543/B543M, Welded ASME SB543; Plate – ASTM B432; Plate & Sheet – for Pressure Vessels, Condensers & Heat Exchangers ASTM B171/B171M, for Pressure Vessels, Condensers & Heat Exchangers ASME SB171; Seamless Condenser Tube & Ferrule Stock – ASTM B111/B111M, ASME SB111; Seamless Heat Exchanger and Condenser Tube - U-Bend ASME SB395, U-Bend ASTM B395/B395M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.53 g/cc0.308 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 7575
Hardness, Rockwell 30T 3737
Tensile Strength 365 MPa53000 psi
Tensile Strength, Yield 152 MPa22000 psi0.5% Ext
Elongation at Break 65 %65 %
Tensile Modulus 110 GPa16000 ksi
Modulus of Rigidity 41.4 GPa6000 ksi
Poissons Ratio 0.330.33Calculated
Machinability 30 %30 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000690 ohm-cm0.00000690 ohm-cm25% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.2 µm/m-°C
@Temperature 20.0 - 300 °C
11.2 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 9.22 W/m-K64.0 BTU-in/hr-ft²-°F
Melting Point 899 - 938 °C1650 - 1720 °F
Solidus 899 °C1650 °F
Liquidus 938 °C1720 °F
Annealing Point 427 - 593 °C800 - 1100 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 649 - 788 °C1200 - 1450 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 70 - 73 %70 - 73 %
Iron, Fe <= 0.060 %<= 0.060 %
Lead, Pb <= 0.070 %<= 0.070 %
Phosphorus, P 0.020 - 0.10 %0.020 - 0.10 %
Tin, Sn 0.80 - 1.2 %0.80 - 1.2 %
Zinc, Zn 25.6 - 29.2 %25.6 - 29.2 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC44500x2 / 292000

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.