MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT Group TuffGel 332 High Strength Silicone Gel
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: TufGel 332 is a clear, tough, moderately cross-linked silicone elastomer, which has good room temperature cure adhesion to many substrates. This material also has enhanced flame retardant properties compared to standard gels. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provide excellent moisture protection.

Key Features:

  • One to one mix ratio
  • High strength
  • Dispensing equipment not necessary
  • Non-yellowing catalyst system
  • Good adhesion to many substrates including glass, aluminum and copper with primer

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/ccUncatalyzed, TufGel 332A
 0.970 g/cc0.970 g/ccUncatalyzed, TufGel 332B
Viscosity 750 cP750 cPUncatalyzed, TufGel 332B
 820 cP820 cPUncatalyzed, TufGel 332A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 30 - 55
@Treatment Temp. 150 °C,
Time 1800 sec
30 - 55
@Treatment Temp. 302 °F,
Time 0.500 hour
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hour
 30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
 60.0 min
@Temperature 100 °C
1.00 hour
@Temperature 212 °F
Gel Time 300 min300 minCatalyzed
 
Descriptive Properties
AppearanceTransparentUncatalyzed, TufGel 332A
 TransparentUncatalyzed, TufGel 332B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QGel 319 Optically Clear Silicone Gel
CHT Group QGel 322 General Purpose Silicone Gel
CHT Group QGel 327 General Purpose Silicone Gel
CHT Group QGel 342 Custom Silicone Gel
Dow Silastic® MEDICAL ADHESIVE SILICONE, TYPE A

PACC2130 / 199518

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.