Eastman Tritan™ Renew TX1000-25 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. This next generation copolyester can also be molded into various applications without incorporating high levels of residual stress. Combined with Eastman Tritan's outstanding chemical resistance and hydrolytic stability, these features give molded products enhanced durability in the dishwasher environment, which can expose products to high heat, humidity and aggressive cleaning detergents. Tritan Renew TX1000-25 may be used in repeated use food contact articles under United States Food and Drug Administration (FDA) regulations. Tritan Renew TX1000-25 is certified to NSF/ANSI Standard 51 for Food Equipment Materials. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation. Applications - Appliances (food contact)
- Building materials
- Compounders
- Consumer housewares-nfc
- Large appliances non-food contact
- Lighting
- Non-medical housings & hardware for electrical
- Small appliances non-food contact
- Water/sport bottles
Key Attributes- Ease of processing
- Excellent clarity
- Excellent hydrolytic stability
- Fast drying times
- Good chemical resistance
- Good heat resistance
- Outstanding impact resistance
- Quick cycle times
Information provided by Eastman. |