Fine weave (less than 4 ounce/square yard) cotton fabric commonly called linen, combined with phenolic resin to provide better machining than BP11NPN. BP21NPN should be used for smaller and more intricate shapes than BP11NPN, when a finer surface finish is required. |
Cotton, Phenolic, Micarta |