LDC800YY is a low density polyethylene resin for extrusion coating and is a barefoot grade. LDC800YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 2.1 & (c) 2.2. Applications: Coating for all substrates Additives: Barefoot Advantages: - Good drawdown
- Good heat seal ability and adhesion properties
Information provided by Titan Chemicals |