MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics Tecknit® 72-00014 Silver-Filled Flexible Resin Caulking System
Categories: Polymer

Material Notes: Description: TECKNIT standard electrically conductive caulks consist of four one-component resin systems filled with silver plated glass or copper particles. These systems are formulated to provide over 100 dB total shielding effectiveness across the RF spectrum. They may be used to improve joint or seam integrity for all types of electronic enclosures. An outstanding feature of these one-component systems is the ease with which they may be applied with conventional caulking guns and dispensing equipment, such as small bead orifice syringes. Hand application with spatula or putty knife is also simple. High yield per pound is another advantage offered in these conductive caulks. Proprietary formulation techniques result in lower density than most current state-of-the-art caulking compounds. The systems are safe to handle, very easily applied and free of any corrosive binders. They contain silver plated glass or copper particles for electrical conductivity, assuring stable operation over wide temperature ranges not generally possible with carbon- black filled systems.

Application Information: This system is a conductive, fast room temperature curing silicone-silver caulking compound. Ease of application and high electrical conductivity are outstanding features of this flexible system. It is used to fill gaps in shielded room joints, repair damaged conductive gaskets and shield/seal permanently mounted panels, components and hardware. This system will withstand shock vibration, seam warping

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Shear Strength >= 0.172 MPaCured; ASTM D1002
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.010 ohm-cmCured; QAP-1017
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °CCured
Minimum Service Temperature, Air -63.0 °CCured
Shrinkage <= 26 %Cured
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
@Temperature 25.0 °C
Recommended Cure
 24.0 hour
@Temperature 25.0 °C
Full Cure
Shelf Life 9.00 MonthUnopened Container
 
Descriptive Properties
ColorTan
ConsistencySelf-Leveling
FillerAg/Glass
Final ConditionFlexible
Number of ComponentsOne
ResinSilicone
Volume13.8 in3
Weight16 oz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHOME405 / 131115

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.