MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sipol Technipol® Bio 1160 Aromatic - Aliphatic Copolyester
Categories: Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Description: Technipol® Bio 1160 is an aromatic - aliphatic copolyester, characterized by medium crystallinity and a low melting point. Due to its formulation, it can be used in biodegradable and compostable compounds. Furthermore it exhibits a good compatibility with other biodegradable polymers as polylactic acid and starch. It can be used as support polymer for master-batches both in granules and in powder form. Usable for injection molding.

Information provided by SIPOL SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D 792
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 160 °C
20 g/10 min
@Load 4.76 lb,
Temperature 320 °F
ASTM D 1238
Storage Temperature 5.00 - 10.0 °C41.0 - 50.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3434instantaneous; ASTM D 2240
Tensile Strength at Break 17.0 MPa2470 psiASTM D 638
Elongation at Break 365 %365 %ASTM D 638
 
Thermal PropertiesMetricEnglishComments
Melting Point 115 °C239 °FASTM D 3418
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIPOL039 / 297164

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.