MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Unifrax Fiberfrax® Pumpable-GS Pumpable Insulation
Categories: Ceramic

Material Notes: Fiberfrax Pumpable-LDS, Pumpable-GS, and Topcoat 2600 Insulating Mix were designed for application into difficult-to-reach areas requiring insulation. Fiberfrax Pumpable-LDS and Pumpable-GS have temperature grade ratings of 1260°C (2300°F). Fiberfrax Topcoat 2600 Insulating Mix has a temperature grade rating of 1426°C (2600°F). A conventional air-operated extrusion pump permits application of these products directly from their container into furnace and boiler hot spots, refractory cracks, furnace door jambs, and other areas requiring high-temperature insulating and sealing.

    Typical Applications
  • On-line boiler hot spot repairs
  • Seal surface door jambs
  • Seal furnace penetrations
  • Seal around burner blocks
  • Caulk refractory cracks
  • On-line refractory hot spot repairs
  • Turbine exhaust duct hot spot repairs

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.400 g/cc0.0145 lb/in³Dry
 1.12 g/cc0.0405 lb/in³Wet
Solids Content 28 %28 %
Loss On Ignition 3.0 - 4.0 %3.0 - 4.0 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00241 GPa0.350 ksiDry
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1093 °C1999 °FRecommended Operating Temperature
Shrinkage 6.0 %
@Temperature 1090 °C,
Time 86400 sec
6.0 %
@Temperature 1990 °F,
Time 24.0 hour
 
Descriptive Properties
AppearanceSmooth putty
Molten Aluminum Wetting ResistanceGood
Temperature Grade (°F)2300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Pumpable-LDS Pumpable Insulation

CUNIF048 / 97820

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.