MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Victrex VICOTE™ F810 Black Polyetheretherketone (PEEK) Liquid Dispersion
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Eco-friendly VICOTE™ Coatings were developed to fill the performance gap found in many existing coating technologies today. Whether applied to industrial, automotive, food processing, semiconductor, electronics or pharmaceutical parts. VICOTE Coatings can be applied using electrostatic or conventional dispersion spray techniques.

The main ingredient of VICOTE Coatings is VICTREX™ PEEK polymer, a linear, aromatic, semi-crystalline thermoplastic, widely regarded as one of the highest performing thermoplastic materials in the world. It offers a unique combination of properties to help processors and end users reach new levels of cost savings, performance, and product differentiation.

These grades have been specifically formulated to provide a resilient coating with varying levels of lubricant to give high wear and abrasion resistance combined with very good release properties. Available in natural and black. Electrostatic dissipative (ESD) grade. All other grades are Insulative coatings.

F-Grades of VICOTE Coatings are specially formulated by Victrex to solve the problem of flash rusting that can occur when water-based coatings are applied to ferrous metals such as mild steel. Can also coat non-ferrous substrates equally effectively.

All information provided by Victrex.

Vendors: With over 30 years of focus, experience and security of supply Victrex Polymer Solutions is the world’s leading manufacturer of high performance Polyaryletherketones (PAEK) including versatile VICTREX™ PEEK. We work with our customers and end users to deliver technology driven solutions to meet the challenges and opportunities they face and help them to achieve new levels of cost savings, quality and performance. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Storage Temperature 5.00 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Impact 1.01m, 1kg, Indent 5mm; ISO 6272
Coefficient of Friction 0.090µm @ 10 min., Using 250N Load; ASTM G 133
 
Processing PropertiesOriginal ValueComments
Drying Temperature 120 °Covernight before use
 150 °C
@Time 10800 sec
 
Descriptive Properties
ColorBlack
Konig Hardness (seconds)120ISO 1522

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 6150 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round

PVICTA42 / 83658

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.