MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT Group QSil FX 22 Shore A, Addition Cure, Translucent Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: Stretch FX is a two-component, room temperature, addition cure, silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for moldmaking of intricate patterns, skin molding and applications where a low durometer translucent material is required.

Key Features:

  • Low viscosity
  • Fast demold time
  • Elongation > 1200%
  • Excellent flexibility
  • Translucent, pigmentable
Main Applications:
  • Special effects
  • Skin replication
  • Applications where pigmentation is required

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccUncatalyzed, Stretch FX B
 1.12 g/cc1.12 g/ccUncatalyzed, Stretch FX A
Viscosity 2000 cP2000 cPUncatalyzed, Stretch FX B
 10000 cP10000 cPCatalyzed
 25000 cP25000 cPUncatalyzed, Stretch FX A
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inCured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2222Cured
Tensile Strength 3.45 MPa500 psiCured
Elongation at Break 1200 %1200 %Cured
Tear Strength 17.5 kN/m100 pliCured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hourDemold
Pot Life 32.0 min32.0 min
 
Descriptive Properties
AppearanceTranslucentUncataylzed, Stretch FX A
 TranslucentUncataylzed, Stretch FX B
 TranslucentCatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PACC2123 / 199511

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.