MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Goodfellow Evanohm® Precision Resistance Nickel Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Nickel Alloy

Material Notes: Electrical resistance alloy with a very low temperature coefficient of resistivity

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.10 g/cc0.293 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1210 MPa175000 psi
Elongation at Break <= 33 %<= 33 %
Tensile Modulus 221 GPa32100 ksi
Izod Impact, Unnotched 0.420 - 1.00 J/cm0.787 - 1.87 ft-lb/inNotch Status Unknown
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000134 ohm-cm0.000134 ohm-cmTemperature Coefficient of 0.00001/K
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.7 µm/m-°C
@Temperature 20.0 - 100 °C
6.50 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 14.6 W/m-K101 BTU-in/hr-ft²-°F
Melting Point 1340 - 1390 °C2440 - 2530 °F
Solidus 1340 °C2440 °F
Liquidus 1390 °C2530 °F
Maximum Service Temperature, Air 300 °C572 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.5 %2.5 %
Chromium, Cr 20 %20 %
Copper, Cu 2.5 %2.5 %
Nickel, Ni 75 %75 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schwarzkopf Plansee PM 1000 ODS Nickel Alloy
Goodfellow Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy
Crucible Compaction Metals P/M 625 Corrosion Resistant Alloy
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Aged 732°C (1350°F)/8hr/AC
Carlson C 601 Nickel-Chromium-Iron Alloy

NGOODF146 / 16218

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.