MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Americhem Engineered Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: 13% glass-filled V-0 rated PBT

All information provided by LTL Color Compounders, Inc. LTL was acquired by Americhem in 2014.

Key Words: PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.53 g/cc1.53 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm0.0050 - 0.0080 in/in0.125 in.; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D785
Tensile Strength at Break 82.7 MPa12000 psi2.0 in/min; ASTM D638
Flexural Strength 145 MPa21000 psi2.0 in/min; ASTM D790
Flexural Modulus 4.34 GPa630 ksi2.0 in/min; ASTM D790
Izod Impact, Notched 0.534 J/cm
@Temperature 22.8 °C
1.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 182 °C360 °FUnannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 243 - 266 °C470 - 510 °F
Middle Barrel Temperature 249 - 271 °C480 - 520 °F
Front Barrel Temperature 254 - 277 °C490 - 530 °F
Nozzle Temperature 249 - 271 °C480 - 520 °F
Melt Temperature 254 - 277 °C490 - 530 °F
Mold Temperature 65.6 - 87.8 °C150 - 190 °F
Drying Temperature 121 °C250 °F
Dry Time 3 - 4 hour3 - 4 hournominal; maximum drying time of 12 hours
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00127 - 0.00254 cm0.000500 - 0.00100 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celanex® 5200-2 PBT, 15% Glass Reinforced
Celanese Celanex® 3300-2LM PBT, Glass Reinforced
BASF Ultradur® S 4090 G6 30% Glass Filled PBT
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber
Plastcom SLOVASTER® B GF 10 Polybutylene Terephthalate, 10% Glass Fiber

PLTLC040 / 104425

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.